Influence of Preliminary Thermomagnetic Treatment on the Yield Point of NaCl:Ni Crystals

The influence of preliminary annealing (3 h, 1000 K), subsequent quenching in liquid nitrogen, and short magnetization in a constant magnetic field (0.5 h, 0.48 T) prior to deformation on the yield point of NaCl : Ni crystals is discovered. The effect depends on the time of sample storage between quenching and magnetization and is maximal 40 h after quenching. © 2003 MAIK "Nauka/Interperiodica".

Авторы
Smirnov A.E.1 , Bekkauer N.N. 2 , Sadchikov V.V.3
Номер выпуска
6
Язык
Английский
Страницы
972-973
Статус
Опубликовано
Том
48
Год
2003
Организации
  • 1 Shubnikov Inst. of Crystallography, Russian Academy of Sciences, Leninskiǐ pr. 59, Moscow, 119333, Russian Federation
  • 2 Peoples Friendship University, ul. Miklukho-Maklaya 6, Moscow, 117198, Russian Federation
  • 3 Bardin Ctrl. Res. Inst. Iron Stl. I., Vtoraya Baumanskaya ul. 9/23, Moscow, 107005, Russian Federation
Ключевые слова
nitrogen; sodium chloride; article; chemical structure; crystallization; decomposition; magnetic field; magnetism; thermodynamics