The influence of the oxidative dehydrogenation of butene-1 on the phase composition of the nickel ferrite/γ-Al2O3 catalyst

The influence of the oxidative dehydrogenation of butene-1 on the phase composition of a ferrite-containing catalyst on γ-Al2O 3 with a Ni: Fe atomic ratio of 1: 4 was studied. It was found by X-ray diffraction, EPR, IR absorption spectroscopy, and derivatography that the reduction of Fe3+ to Fe2+ with the formation of The Fe3O4 magnetite phase occurred under various conditions of olefin (reaction mixture)-catalyst surface contact. The treatment of the catalyst with the reaction mixture and its oxidation decrease the degree of spinel phase imperfection. © Nauka/Interperiodica 2006.

Авторы
Eyubova S.M.1 , Amirbekov A.N.1 , Mamedova S.A.1 , Aliev F.V.1 , Yagodovskii V.D. 2
Номер выпуска
1
Язык
Английский
Страницы
68-71
Статус
Опубликовано
Том
80
Год
2006
Организации
  • 1 Mamedaliev Institute of Petrochemical Processes, Academy of Sciences of Azerbaijan, Baku, Azerbaijan
  • 2 Russian University of Peoples' Friendship, ul. Miklukho-Maklaya 6, Moscow, 117198, Russian Federation
Ключевые слова
Absorption spectroscopy; Butenes; Catalysts; Oxidation; Phase composition; X ray diffraction; Derivatography; Reaction mixtures; Surface contact; Dehydrogenation